Type | MgO | SiO2 | Al2O3 | CaO | Fe2O3 |
M type | ≥97.5 | ≤0.70 | ≤0.10 | ≤1.10 | ≤0.46 |
MA type | ≥74.5 | ≤0.74 | ≤22.2 | ≤1.20 | ≤0.51 |
Type | Porosity | Cold crushing strength Mpa | Coefficient of thermal expansion 20-1300C | Resistance to urgent cold urgent heat times N 1200C | Bulk density Kg/m3 | Max working temperature C 0.13pa |
M type | 14/19 | ≥19.6 | ≤13×10-6 | ≥40 | 2.9/3.1×103 | 1750 |
MA type | 18/22 | ≥14.7 | ≤9×10-6 | ≥40 | 2.8/3.05×103 | 1750 |
Features:
1. High temperature resistance
2. Wear resistance
3. Corrosion resistance
4. Acid and alkali resistant
5. Resistance to compression
6. Good thermal stability